Why the electric furnace internal severe crack in the wall part?
As shown in figure: the furnace is sintering of zirconia ceramics, using temperature at 1500 ℃, but the furnace has two obvious defect without air intake and air flow. Ceramic raw embryo generally contains 1 ~ 5% of organic matter, organic matter under 600 ℃ will discharge, but without inlet and vent, excluded from organic matter (contain K, Na) would be absorbed by the chamber of a stove or furnace material, the high temperature will be severe cracking furnace and furnace material reaction materials, because of the organic matter density than air, so in the chamber of a stove or furnace part of cracks are more serious.
“推荐阅读”
- Why first use of ceramic fiber textile will turn black?
- Why a circle appears on the furnace door, and black?
- The chamber of a stove or furnace wall crack, how to deal with?
- High temperature industrial furnace heat insulating varnish insulation effect
- The chemical reaction principle of the experimental furnace gasification stage
- In today's society is analysed high performance refractories greater development potential
- Science and technology innovation to accelerate the development of refractory industry
- The selection of insulating refractory application in metallurgical industry
- ALCERA - high-end thermal insulation material manufacturers
- "ALCERA" VOC waste gas purification furnace is introduced